English French German Portuguese Spanish Russian Japanese Korean Arabic Irish Greek Turkish Italian Danish Romanian Indonesian Czech Afrikaans Swedish Polish Basque Catalan Esperanto Hindi Lao Albanian Amharic Armenian Azerbaijani Belarusian Bengali Bosnian Bulgarian Cebuano Chichewa Corsican Croatian Dutch Estonian Filipino Finnish Frisian Galician Georgian Gujarati Haitian Hausa Hawaiian Hebrew Hmong Hungarian Icelandic Igbo Javanese Kannada Kazakh Khmer Kurdish Kyrgyz Latin Latvian Lithuanian Luxembou.. Macedonian Malagasy Malay Malayalam Maltese Maori Marathi Mongolian Burmese Nepali Norwegian Pashto Persian Punjabi Serbian Sesotho Sinhala Slovak Slovenian Somali Samoan Scots Gaelic Shona Sindhi Sundanese Swahili Tajik Tamil Telugu Thai Ukrainian Urdu Uzbek Vietnamese Welsh Xhosa Yiddish Yoruba Zulu Kinyarwanda Tatar Oriya Turkmen Uyghur Abkhaz Acehnese Acholi Alur Assamese Awadish Aymara Balinese Bambara Bashkir Batak Karo Bataximau Longong Batak Toba Pemba Betawi Bhojpuri Bicol Breton Buryat Cantonese Chuvash Crimean Tatar Sewing Divi Dogra Doumbe Dzongkha Ewe Fijian Fula Ga Ganda (Luganda) Guarani Hakachin Hiligaynon Hunsrück Iloko Pampanga Kiga Kituba Konkani Kryo Kurdish (Sorani) Latgale Ligurian Limburgish Lingala Lombard Luo Maithili Makassar Malay (Jawi) Steppe Mari Meitei (Manipuri) Minan Mizo Ndebele (Southern) Nepali (Newari) Northern Sotho (Sepéti) Nuer Occitan Oromo Pangasinan Papiamento Punjabi (Shamuki) Quechua Romani Rundi Blood Sanskrit Seychellois Creole Shan Sicilian Silesian Swati Tetum Tigrinya Tsonga Tswana Twi (Akan) Yucatec Maya
Inquiry
Form loading...

Iyọọda bàbà-nickel-beryllium C17510

C17510 alloy copper-nickel-beryllium, tí a tún mọ̀ sí CuNi2Be, idẹ beryllium àti copper ìgbà ìrúwé, jẹ́ àdàpọ̀ bàbà pẹ̀lú 0.2–0.6% beryllium, 1.4-2.2% nickel àti nígbà míìrán àwọn èròjà míràn.

  • Ìmọ̀-ẹ̀rọ Ìbámu
  • Ìfìṣọ̀kan Ó dára
  • Fífúnni ní àwo Ó dára
  • Alurinmorin Oxyacetylene A ko ṣeduro
  • Alurinmorin Arc ti a Daabo Bo Gaasi Dáradára
  • Alurinmorin Arc Irin ti a fi bo Dáradára

Ifihan

C17510 alloy copper-nickel-beryllium, tí a tún mọ̀ sí CuNi2Be, idẹ beryllium àti copper ìgbà ìrúwé, jẹ́ àdàpọ̀ bàbà pẹ̀lú 0.2–0.6% beryllium, 1.4-2.2% nickel àti nígbà míìrán àwọn èròjà míràn.

Iyọọda bàbà-nickel-beryllium C17510 Ó so agbára gíga pọ̀ mọ́ àwọn ànímọ́ tí kì í ṣe magnetic àti èyí tí kì í mú kí iná mànàmáná jáde. Ó ní àwọn ànímọ́ iṣẹ́ irin tó dára, ìṣẹ̀dá àti iṣẹ́ ẹ̀rọ tó dára.

C17510, alloy copper-nickel-beryllium kan, pese agbara to dara pelu agbara itanna ati ooru giga, resistance to dara si isinmi wahala ati agbara otutu to ga. A ṣe alloy c17510 fun iṣẹ to dara julọ ni thàwọn ilé iṣẹ́ ọkọ̀ ayọ́kẹ́lẹ́, ìbánisọ̀rọ̀ àti epo àti gaasi.

Àwọn Ànímọ́ Ti Ara:

Aaye Yíyọ́ - Liquidus°F 1955
Aaye Yíyọ́ - Solidus°F 1885
Dínsitylb/cu in. ní 68°F 0.317
Wíwúwo pàtó 8.77
Ìgbékalẹ̀ Iná Mànàmáná% IACS ní 68°F 48 (1)
Ìgbékalẹ̀ Iná Mànàmáná% IACS ní 68°F 45 (2)
Ìgbékalẹ̀ Ìgbóná Btu/ sq ft/ ft hr/ °F ní 68°F 120
Ìṣọ̀kan Ìfẹ̀sí-ooru 68-39210⁻⁶ fún °F (68 – 392°F) 9.8
Agbara Ooru Kan patoBtu/ lb /°F ni 68°F 0.1
Modulu ti Elasticity ninu Tension/ksi 19200
Modulu ti Rigidity/ksi 7500

(1) Iṣẹ́ tútù àti ipò òjò líle. HT Temper

(2) AT Temper